MECHSOLVER

Ti-6Al-4V (Grade 5 Titanium) vs Al 7075-T6 Comparison

ASTM B348 / AMS 4928ASTM B221 / AMS 4123

Ti-6Al-4V (Grade 5) delivers 880 MPa yield strength, 400 °C heat capability, and exceptional fatigue/corrosion resistance, while Al 7075-T6 matches specific stiffness (E/ρ) at a fraction of the material and CNC machining cost.

Primary Engineering Specifications

Material A
Ti-6Al-4V (Grade 5 Titanium)
Yield Strength (Re)
880 MPa
Tensile Strength (Rm)
950 MPa
Elastic Modulus (E) / Density
114 GPa / 4.43 g/cm³
Typical Hardness
36 HRC
Weldability / Thermal
Weldable with strict argon shielding
Machinability
Difficult (low thermal conductivity, slow speeds)

Al 7075-T6

Material B
Al 7075-T6
Yield Strength (Re)
503 MPa
Tensile Strength (Rm)
572 MPa
Elastic Modulus (E) / Density
71.7 GPa / 2.81 g/cm³
Typical Hardness
150 HB
Weldability / Thermal
Not weldable
Machinability
Excellent (high-speed CNC)

Design & Manufacturing Note

Choose Al 7075-T6 for lightweight CNC structures below 120 °C; upgrade to Ti-6Al-4V when elevated temperature, corrosion/biocompatibility, or extreme compact strength governs.

Frequently Asked Questions

Which is stronger: Ti-6Al-4V or Al 7075-T6?

Ti-6Al-4V (Grade 5 Titanium) has a typical yield strength of 880 MPa (tensile 950 MPa), while Al 7075-T6 provides 503 MPa yield (tensile 572 MPa).

When should I choose Ti-6Al-4V over Al 7075-T6?

Choose Al 7075-T6 for lightweight CNC structures below 120 °C; upgrade to Ti-6Al-4V when elevated temperature, corrosion/biocompatibility, or extreme compact strength governs.