AISI 4140 (42CrMo4) vs AISI 4340 (34CrNiMo6) Comparison

EN 10083-3 / ASTM A29EN 10083-3 / AMS 6415

AISI 4140 (42CrMo4) and AISI 4340 (34CrNiMo6) are quenched-and-tempered alloy steels; 4340’s nickel content delivers superior through-hardenability and impact toughness in heavy sections, while 4140 offers lower cost and better machinability for general shafts and gears.

Primary Engineering Specifications

Material A
AISI 4140 (42CrMo4)
Yield Strength (Re)
655 MPa (QT)
Tensile Strength (Rm)
1000 MPa (QT)
Elastic Modulus (E) / Density
210 GPa / 7.85 g/cm³
Typical Hardness
28–34 HRC
Weldability / Thermal
Requires preheat (250–350 °C)
Machinability
Moderate (65% of AISI 1212)

AISI 4340 (34CrNiMo6)

Material B
AISI 4340 (34CrNiMo6)
Yield Strength (Re)
860 MPa (QT)
Tensile Strength (Rm)
1080–1200 MPa (QT)
Elastic Modulus (E) / Density
205 GPa / 7.85 g/cm³
Typical Hardness
32–40 HRC
Weldability / Thermal
Difficult (high preheat + PWHT)
Machinability
Low–Moderate (50% of AISI 1212)

Design & Manufacturing Note

Choose 4140 for general shafts, spindles, and sections under ~80 mm where cost and machinability matter; upgrade to 4340 for heavy cross-sections (Ø100+ mm), high-impact shock loads, and aerospace/critical drive shafts.

Frequently Asked Questions

Which is stronger: AISI 4140 or AISI 4340?

AISI 4140 (42CrMo4) has a typical yield strength of 655 MPa (QT) (tensile 1000 MPa (QT)), while AISI 4340 (34CrNiMo6) provides 860 MPa (QT) yield (tensile 1080–1200 MPa (QT)).

When should I choose AISI 4140 over AISI 4340?

Choose 4140 for general shafts, spindles, and sections under ~80 mm where cost and machinability matter; upgrade to 4340 for heavy cross-sections (Ø100+ mm), high-impact shock loads, and aerospace/critical drive shafts.