S355J2 (St52) delivers 51% higher yield strength than S235JR (355 MPa vs 235 MPa) plus guaranteed -20 °C impact toughness (27 J), while both steels share the exact same elastic modulus (210 GPa).
S235JR (St37) vs S355J2 (St52) Comparison
EN 10025-2EN 10025-2
Primary Engineering Specifications
- Material A
- S235JR (St37)
- Yield Strength (Re)
- 235 MPa
- Tensile Strength (Rm)
- 360–510 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 110–140 HB
- Weldability / Thermal
- Excellent (no preheat)
- Machinability
- Good (soft, slightly gummy)
S355J2 (St52)
- Material B
- S355J2 (St52)
- Yield Strength (Re)
- 355 MPa
- Tensile Strength (Rm)
- 470–630 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 145–185 HB
- Weldability / Thermal
- Very good (light preheat on thick plates)
- Machinability
- Good (cleaner chip breaking)
Design & Manufacturing Note
Pick S355J2 when stress/yield governs or cold-weather toughness is required; pick S235JR when deflection/stiffness governs (identical E = 210 GPa) or for lightly loaded brackets and guards.
Frequently Asked Questions
Which is stronger: S235JR or S355J2?
S235JR (St37) has a typical yield strength of 235 MPa (tensile 360–510 MPa), while S355J2 (St52) provides 355 MPa yield (tensile 470–630 MPa).
When should I choose S235JR over S355J2?
Pick S355J2 when stress/yield governs or cold-weather toughness is required; pick S235JR when deflection/stiffness governs (identical E = 210 GPa) or for lightly loaded brackets and guards.