C45 (1045) is an unalloyed medium-carbon steel whereas 42CrMo4 (4140) is a Cr-Mo alloy steel offering nearly double the quenched-and-tempered yield strength and far higher fatigue resistance for heavily loaded shafts and gears.
C45 (AISI 1045) vs 42CrMo4 (AISI 4140) Comparison
EN 10083-2EN 10083-3
Primary Engineering Specifications
- Material A
- C45 (AISI 1045)
- Yield Strength (Re)
- 370–490 MPa
- Tensile Strength (Rm)
- 620–750 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 180–225 HB
- Weldability / Thermal
- Limited (requires preheat)
- Machinability
- Good (65%)
42CrMo4 (AISI 4140)
- Material B
- 42CrMo4 (AISI 4140)
- Yield Strength (Re)
- 655–750 MPa
- Tensile Strength (Rm)
- 900–1100 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 280–330 HB
- Weldability / Thermal
- Difficult (250–350 °C preheat + temper)
- Machinability
- Moderate (55–65%)
Design & Manufacturing Note
Use C45 for moderately loaded shafts, bushings, and cost-sensitive induction-hardened parts; choose 42CrMo4 for high-torque gearbox shafts, severe fatigue cycles, and thick quenched-and-tempered sections.
Frequently Asked Questions
Which is stronger: C45 or 42CrMo4?
C45 (AISI 1045) has a typical yield strength of 370–490 MPa (tensile 620–750 MPa), while 42CrMo4 (AISI 4140) provides 655–750 MPa yield (tensile 900–1100 MPa).
When should I choose C45 over 42CrMo4?
Use C45 for moderately loaded shafts, bushings, and cost-sensitive induction-hardened parts; choose 42CrMo4 for high-torque gearbox shafts, severe fatigue cycles, and thick quenched-and-tempered sections.