POM-C (Acetal/Delrin) offers superior dimensional stability (<0.2% moisture absorption) and crisp CNC machinability, whereas PA6 (Nylon 6) provides higher impact toughness and abrasion resistance at the cost of moisture swelling.
POM-C (Delrin / Acetal) vs PA6 (Polyamide / Nylon 6) Comparison
ISO 29988ISO 16396
Primary Engineering Specifications
- Material A
- POM-C (Delrin / Acetal)
- Yield Strength (Re)
- 65 MPa
- Tensile Strength (Rm)
- 65–70 MPa
- Elastic Modulus (E) / Density
- 2.8–3.1 GPa / 1.41 g/cm³
- Typical Hardness
- 80–85 Shore D
- Weldability / Thermal
- Heat / ultrasonic weldable
- Machinability
- Excellent (premier CNC plastic)
PA6 (Polyamide / Nylon 6)
- Material B
- PA6 (Polyamide / Nylon 6)
- Yield Strength (Re)
- 75–85 MPa (dry)
- Tensile Strength (Rm)
- 75–85 MPa
- Elastic Modulus (E) / Density
- 3.0 GPa (dry) / 1.5 GPa (wet) / 1.14 g/cm³
- Typical Hardness
- 78–82 Shore D
- Weldability / Thermal
- Suitable for vibration/hot-plate welding
- Machinability
- Good (sharp tools, control heat)
Design & Manufacturing Note
Select POM for tight-tolerance gears, bushings, and wet environments; select PA6 (or cast PA6G) for shock-loaded wear pads, sheaves, and heavy conveyor guides.
Frequently Asked Questions
Which is stronger: POM-C or PA6?
POM-C (Delrin / Acetal) has a typical yield strength of 65 MPa (tensile 65–70 MPa), while PA6 (Polyamide / Nylon 6) provides 75–85 MPa (dry) yield (tensile 75–85 MPa).
When should I choose POM-C over PA6?
Select POM for tight-tolerance gears, bushings, and wet environments; select PA6 (or cast PA6G) for shock-loaded wear pads, sheaves, and heavy conveyor guides.