MECHSOLVER

Al 6061-T6 (EN AW-6061) vs Al 7075-T6 (EN AW-7075) Comparison

ASTM B221 / EN 573-3ASTM B221 / EN 573-3

Al 7075-T6 delivers steel-like 503 MPa yield strength at one-third the weight of steel but is non-weldable and less corrosion-resistant; Al 6061-T6 offers 276 MPa yield with good weldability, corrosion resistance, and lower cost.

Primary Engineering Specifications

Material A
Al 6061-T6 (EN AW-6061)
Yield Strength (Re)
276 MPa
Tensile Strength (Rm)
310 MPa
Elastic Modulus (E) / Density
69 GPa / 2.70 g/cm³
Typical Hardness
95 HB
Weldability / Thermal
Good (TIG/MIG weldable)
Machinability
Very good

Al 7075-T6 (EN AW-7075)

Material B
Al 7075-T6 (EN AW-7075)
Yield Strength (Re)
503 MPa
Tensile Strength (Rm)
572 MPa
Elastic Modulus (E) / Density
71.7 GPa / 2.81 g/cm³
Typical Hardness
150 HB
Weldability / Thermal
Not recommended for fusion welding
Machinability
Excellent (crisp chips)

Design & Manufacturing Note

Choose 6061-T6 for welded frames, automation housings, and anodized general CNC parts; choose 7075-T6 for bolted high-stress robotics arms, aerospace fittings, and tooling plates.

Frequently Asked Questions

Which is stronger: Al 6061-T6 or Al 7075-T6?

Al 6061-T6 (EN AW-6061) has a typical yield strength of 276 MPa (tensile 310 MPa), while Al 7075-T6 (EN AW-7075) provides 503 MPa yield (tensile 572 MPa).

When should I choose Al 6061-T6 over Al 7075-T6?

Choose 6061-T6 for welded frames, automation housings, and anodized general CNC parts; choose 7075-T6 for bolted high-stress robotics arms, aerospace fittings, and tooling plates.