16MnCr5 is a case-hardening steel reaching 58–62 HRC on the flank with a tough core—ideal for heavily loaded gears—while 42CrMo4 is a through-hardening steel suited for high-torque shafts and induction-hardened pinions.
16MnCr5 (1.7131 — Case-Hardening) vs 42CrMo4 (1.7225 — Q&T Alloy) Comparison
EN 10084EN 10083-3
Primary Engineering Specifications
- Material A
- 16MnCr5 (1.7131 — Case-Hardening)
- Yield Strength (Re)
- 590–650 MPa (core)
- Tensile Strength (Rm)
- 800–1100 MPa (core)
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 58–62 HRC (case)
- Weldability / Thermal
- Good before carburizing
- Machinability
- Very good when soft-annealed
42CrMo4 (1.7225 — Q&T Alloy)
- Material B
- 42CrMo4 (1.7225 — Q&T Alloy)
- Yield Strength (Re)
- 655–750 MPa
- Tensile Strength (Rm)
- 900–1100 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 28–34 HRC (core) / 52–56 HRC (induction)
- Weldability / Thermal
- Difficult (preheat required)
- Machinability
- Moderate
Design & Manufacturing Note
Select 16MnCr5 for high-load carburized gears and cams where pitting governs; select pre-hardened 42CrMo4 for long precision shafts where carburizing distortion must be avoided.
Frequently Asked Questions
Which is stronger: 16MnCr5 or 42CrMo4?
16MnCr5 (1.7131 — Case-Hardening) has a typical yield strength of 590–650 MPa (core) (tensile 800–1100 MPa (core)), while 42CrMo4 (1.7225 — Q&T Alloy) provides 655–750 MPa yield (tensile 900–1100 MPa).
When should I choose 16MnCr5 over 42CrMo4?
Select 16MnCr5 for high-load carburized gears and cams where pitting governs; select pre-hardened 42CrMo4 for long precision shafts where carburizing distortion must be avoided.