MECHSOLVER

AISI 304 (1.4301) vs AISI 316 (1.4401 / 316L) Comparison

EN 10088 / ASTM A240EN 10088 / ASTM A240

AISI 304 and AISI 316 have nearly identical mechanical strength, but 316’s 2–3% molybdenum addition dramatically improves resistance to chloride pitting in marine, chemical, and food-brine environments.

Primary Engineering Specifications

Material A
AISI 304 (1.4301)
Yield Strength (Re)
215 MPa
Tensile Strength (Rm)
505 MPa
Elastic Modulus (E) / Density
193 GPa / 8.00 g/cm³
Typical Hardness
170–200 HB
Weldability / Thermal
Excellent (use 304L to prevent sensitization)
Machinability
Moderate (work-hardens; sharp tooling needed)

AISI 316 (1.4401 / 316L)

Material B
AISI 316 (1.4401 / 316L)
Yield Strength (Re)
205–240 MPa
Tensile Strength (Rm)
515–580 MPa
Elastic Modulus (E) / Density
193 GPa / 8.00 g/cm³
Typical Hardness
170–215 HB
Weldability / Thermal
Excellent (316L preferred)
Machinability
Fair (slightly tougher than 304)

Design & Manufacturing Note

Use 304 for indoor food equipment, guards, and general corrosion protection; specify 316/316L for marine exposure, chlorides, brine, and pharmaceutical or chemical piping.

Frequently Asked Questions

Which is stronger: AISI 304 or AISI 316?

AISI 304 (1.4301) has a typical yield strength of 215 MPa (tensile 505 MPa), while AISI 316 (1.4401 / 316L) provides 205–240 MPa yield (tensile 515–580 MPa).

When should I choose AISI 304 over AISI 316?

Use 304 for indoor food equipment, guards, and general corrosion protection; specify 316/316L for marine exposure, chlorides, brine, and pharmaceutical or chemical piping.