While C45 and S355J2 overlap in normalized yield strength, S355J2 is engineered for welded structural frames with low carbon equivalent, whereas C45 is a machining and heat-treatable steel for shafts, keys, and gears.
C45 (1.0503) vs S355J2 (1.0577) Comparison
EN 10083-2EN 10025-2
Primary Engineering Specifications
- Material A
- C45 (1.0503)
- Yield Strength (Re)
- 370–490 MPa
- Tensile Strength (Rm)
- 620–750 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 180–225 HB
- Weldability / Thermal
- Poor (preheat + low-hydrogen filler)
- Machinability
- Good (tailored for machining)
S355J2 (1.0577)
- Material B
- S355J2 (1.0577)
- Yield Strength (Re)
- 355 MPa
- Tensile Strength (Rm)
- 470–630 MPa
- Elastic Modulus (E) / Density
- 210 GPa / 7.85 g/cm³
- Typical Hardness
- 145–185 HB
- Weldability / Thermal
- Very good
- Machinability
- Good
Design & Manufacturing Note
Always choose S355J2 if the part will be welded; choose C45 for non-welded machined shafts, parallel keys, and parts requiring flame/induction hardening.
Frequently Asked Questions
Which is stronger: C45 or S355J2?
C45 (1.0503) has a typical yield strength of 370–490 MPa (tensile 620–750 MPa), while S355J2 (1.0577) provides 355 MPa yield (tensile 470–630 MPa).
When should I choose C45 over S355J2?
Always choose S355J2 if the part will be welded; choose C45 for non-welded machined shafts, parallel keys, and parts requiring flame/induction hardening.